China Rare Earth Magnet Limited Manufacturer Neodymium Magnets with Everlube or Nicu+Everlube Coating
|
|
Everlube is a thermosetting coating. Its main components include PTFE, molybdenum disulfide (MoS2) and phenolic resin adhesives. Due to its excellent performance, Everlube coated magnets have become a designated coating for customers at home and abroad. Advantages of Everlube Coating 1. High load 2. Reduce the coefficient of friction; 3. High temperature resistance; 4. Improve chemical resistance; Comparison with conventional rare earth magnet coatings: 1. The Everlube coating has excellent corrosion resistance. 2. Everlube coated magnets are incredibly chemically stable. It can work stably under a simple solvent. 3. Excellent performance in PCT/HAST test, salt spray test and constant temperature and humidity test Application of Everlube Coated Magnets 1. Various permanent magnet motors, such as lifts, servo motors. 2. A variety of generators, such as wind turbines and hydro-electric machines. 3. Automotive industry. We are top neodymium magnets manufacturer in China, welcome to send your inquiry about permanent magnets with Everlube coating by email, we will reply you within one working day |
|
Introduction of Everlube & Nicu+Everlube |
Compare Item |
Everlube |
Nicu+Everlube |
Minimum local thickness (μm) |
8 |
12 |
Neutral salt spray test (H) |
48 |
96 |
Humid Heat test(H) |
240 |
500 |
Pressure cooker test (PCT)(H) |
72 |
120 |
Recommended operating temperature (℃) |
<160 |
<160 |
For what magnet |
There is not special provisions in our company and we commonly recommend plating according to customers' demands. |
There is not special provisions in our company and we commonly recommend plating according to customers' demands. |
Material of the plating |
PTFE, molybdenum ,resin, pigments, organic compounds etc. |
PTFE, molybdenum ,nickel, copper, resin, pigments, organic compounds etc. |
Process of surface treatment technology |
surface ash-removing treatment-phosphorization-flame plating everlube-solidification |
surface ash-removing treatment-electroplate NiCu-phosphorization-flame plating everlube-solidification |
Advantages |
nonmetal and non-conduction plating |
It's salt mist endurance, PCT and ability of humid heat test are all superior than other plating in our company. |
Tags: neodymium magnets, neodymium magnet coating